Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.320 - 1.14 J/g-°C | 0.0765 - 0.272 BTU/lb-°F | Average value: 0.864 J/g-°C Grade Count:15 |
Overview of materials for Silicone, Molded, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val.. |
|||
Specific Heat Capacity | 0.320 - 1.26 J/g-°C | 0.0765 - 0.301 BTU/lb-°F | Average value: 0.789 J/g-°C Grade Count:20 |
Overview of materials for Silicone Rubber This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Specific Heat Capacity | 0.320 J/g-°C | 0.0765 BTU/lb-°F | |
Indium Corp. Germanium Corporation® Germanium Metal Germanium is a hard, brittle, grayish white element. It is transparent to infrared light, which makes it useful for optical materials. It is widely used as a semiconductor and an alloying agent. .. |
|||
Specific Heat Capacity | 0.320 J/g-°C | 0.0765 BTU/lb-°F | |
Hippe PEEK Polyetheretherketone PEEK is a crystalline, easily machinable thermoplastic which is characterized by high tensile and constant good electrical properties between 0°-220°C, as well as due to favorable tribological beh.. |
|||
Specific Heat Capacity | 0.320 - 0.370 J/g-°C | 0.0765 - 0.0884 BTU/lb-°F | |
ETREMA Products Terfenol-D Magnetostrictive Smart Material (Tb0.3Dy0.7Fe1.92) Terfenol-D is the commercial name for Tb0.3Dy0.7Fe1.92; a composition of material that exhibits giant magnetostriction.Magnetostriction is the phenomenon in which an applied magnetic field causes an.. |
|||
Specific Heat Capacity | 0.320 J/g-°C @Temperature 1227 °C |
0.0765 BTU/lb-°F @Temperature 2241 °F |
|
ATI Wah Chang Niobium Niobium is a soft, ductile metal which can be cold worked over 90 percent before annealing becomes necessary. In appearance, the metal is somewhat similar to stainless steel. The density of 8.57 gm/.. |
|||
Specific Heat Capacity | 0.320 J/g-°C | 0.0765 BTU/lb-°F | ASTM E 1461-01 |
Arlon R36133N062 0.062" (1.57 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Layer 1: Cured Silicone Rubber Interleave: Polyethylene This data represents typical values for the production ma.. |