Thermal Properties Metric English Comments
Specific Heat Capacity 0.260 J/g-°C
0.0621 BTU/lb-°F
A Instruments Model 2920 modulated DSC, ASTM TM E1269.
DuPont™ Nomex® 455 (NOMEX III) Aramid Staple Fiber
Type 455 staple of NOMEX, a patented blend of NOMEX and KEVLAR brand fibers, was introduced to fill the need for higher performance thermal protective apparel. Type 450 staple. However, because of..
Specific Heat Capacity 0.260 J/g-°C
0.0621 BTU/lb-°F
A Instruments Model 2920 modulated DSC, ASTM TM E1269.
DuPont™ Nomex® 462 (NOMEX IIIA) Aramid Staple Fiber
Type 462 staple of NOMEX is a blend of NOMEX and KEVLAR brand fibers and P-140, a proprietary static dissipative fiber. When converted to fabric it is known commercially as NOMEX IIIA and is used f..
Specific Heat Capacity 0.260 J/g-°C
0.0621 BTU/lb-°F
CMW® THERMKON® 65M Molybdenum Copper parts
For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc.