Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.047 J/g-°C | 0.2502 BTU/lb-°F | |
Zircar Refractory Composites RS-99M Refractory Sheet Type RS-99M is a plastic highly moldable sheet ideally suited for forming custom geometries.Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI) |
|||
Specific Heat Capacity | 1.047 J/g-°C | 0.2502 BTU/lb-°F | |
Zircar Refractory Composites RS-99R Refractory Sheet Type RS-99R boards are prefired and are unaffected by moisture. They stay rigid even if saturated with water.Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI) |
|||
Specific Heat Capacity | 1.047 J/g-°C | 0.2502 BTU/lb-°F | |
Zircar Refractory Composites RS-99W Refractory Sheet Type RS-99W boards can be moistened with water and molded into any desired shape. After low temperature bake-out of 300°C (570°F) boards are unaffected by moisture.Information provided by ZIRCAR R.. |
|||
Specific Heat Capacity | 1.047 J/g-°C | 0.2502 BTU/lb-°F | |
Zircar Refractory Composites RS-A Refractory Sheet ZRCI`s Refractory Sheet Type RS-A Moldable is a tough ceramic fiber reinforced insulation which contains no asbestos. Developed as an asbestos board replacement for induction coil liners and molten .. |
|||
Specific Heat Capacity | 1.047 J/g-°C | 0.2502 BTU/lb-°F | |
Zircar Refractory Composites RS-A1 Refractory Sheet This product is made from Type RS-A Moldable. Type RS-A was developed as an asbestos board replacement for induction coil liners and molten metal transport, and contains no asbestos. Refractory Shee.. |
|||
Specific Heat Capacity | 1.047 J/g-°C | 0.2502 BTU/lb-°F | |
Zircar Refractory Composites RS-A2 Refractory Sheet This product is made from Type RS-A Moldable. Type RS-A was developed as an asbestos board replacement for induction coil liners and molten metal transport, and contains no asbestos. Refractory Shee.. |
|||
Specific Heat Capacity | 1.047 J/g-°C | 0.2502 BTU/lb-°F | |
Zircar Refractory Composites RS-A3 Refractory Sheet This product is made from Type RS-A Moldable. Type RS-A was developed as an asbestos board replacement for induction coil liners and molten metal transport, and contains no asbestos. Refractory Shee.. |
|||
Specific Heat Capacity | 1.047 J/g-°C | 0.2502 BTU/lb-°F | |
Zircar Refractory Composites RSMAT-3000 ALUMINA MAT ZRCI Type RSMAT-3000 is a high purity, high temperature, flexible form composed of continuous 97% alumina ceramic fibers designed for use to 1650°C (3002°F). Type RSMAT-3000 contains little shot a.. |