Zircar Refractory Composites RS-99M Refractory Sheet

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Zircar Refractory Composites, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zircar Refractory Composites RS-99M Refractory Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type RS-99M is a plastic highly moldable sheet ideally suited for forming custom geometries.Information provided by ZIRCAR Refractory Composites, Inc. (ZRCI)
Physical Properties Metric English Comments
Density 1.70 g/cc
0.0614 lb/in³
Loss On Ignition 4.0 - 5.0 %
4.0 - 5.0 %
Porosity 56 %
56 %
Thermal Properties Metric English Comments
Specific Heat Capacity 1.047 J/g-°C
0.2502 BTU/lb-°F
Melting Point >= 1800 °C
>= 3270 °F
Maximum Service Temperature, Air 1650 °C
3000 °F
Shrinkage 0.400 - 1.00 %

@Temperature 1200 °C,
Time 3600 sec
0.400 - 1.00 %

@Temperature 2190 °F,
Time 1.00 hour
4.00 - 5.00 %

@Temperature 1200 °C,
Time 3600 sec
4.00 - 5.00 %

@Temperature 2190 °F,
Time 1.00 hour
8.00 - 10.0 %

@Temperature 1600 °C,
Time 3600 sec
8.00 - 10.0 %

@Temperature 2910 °F,
Time 1.00 hour
Component Elements Properties Metric English Comments
Al2O3 >= 99 %
>= 99 %
Descriptive Properties Value Comments
Color White