Polymer Property : Specific Heat Capacity = 0.159 BTU/lb-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 0.667 J/g-°C

@Temperature 1100 °C
0.159 BTU/lb-°F

@Temperature 2010 °F
Haynes HR-120® alloy, solution heat-treated
Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts ..
Specific Heat Capacity 0.667 J/g-°C

@Temperature 1100 °C
0.159 BTU/lb-°F

@Temperature 2010 °F
Haynes HR-120® alloy, solution heat-treated aged at 1200°F for 1000 hours
Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts ..
Specific Heat Capacity 0.667 J/g-°C

@Temperature 1100 °C
0.159 BTU/lb-°F

@Temperature 2010 °F
Haynes HR-120® alloy, solution heat-treated aged at 1400°F for 1000 hours
Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts ..
Specific Heat Capacity 0.667 J/g-°C

@Temperature 1100 °C
0.159 BTU/lb-°F

@Temperature 2010 °F
Haynes HR-120® alloy, solution heat-treated aged at 1600°F for 1000 hours
Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts ..
Specific Heat Capacity 0.667 J/g-°C

@Temperature 1100 °C
0.159 BTU/lb-°F

@Temperature 2010 °F
Haynes HR-120® alloy, solution heat-treated aged at 1800°F for 1000 hours
Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts ..
Specific Heat Capacity 0.667 J/g-°C

@Temperature 1100 °C
0.159 BTU/lb-°F

@Temperature 2010 °F
Haynes HR-120® alloy, solution heat-treated plate
Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts ..
Specific Heat Capacity 0.665 J/g-°C
0.159 BTU/lb-°F
ASTM E1269
CoorsTek Pure SiC™ HR CVD Silicon Carbide, > 99.9995%
Data Provided by the manufacturer, CoorsTek, Inc.
Specific Heat Capacity 0.665 J/g-°C
0.159 BTU/lb-°F
ASTM E1269
CoorsTek Pure SiC™ LR CVD Silicon Carbide, > 99.9995%
Data Provided by the manufacturer, CoorsTek, Inc.