Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.660 J/g-°C @Temperature 900 °C |
0.158 BTU/lb-°F @Temperature 1650 °F |
|
Haynes HR-120® alloy, solution heat-treated Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Specific Heat Capacity | 0.663 J/g-°C @Temperature 1000 °C |
0.158 BTU/lb-°F @Temperature 1830 °F |
|
Haynes HR-120® alloy, solution heat-treated Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Specific Heat Capacity | 0.660 J/g-°C @Temperature 900 °C |
0.158 BTU/lb-°F @Temperature 1650 °F |
|
Haynes HR-120® alloy, solution heat-treated aged at 1200°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Specific Heat Capacity | 0.663 J/g-°C @Temperature 1000 °C |
0.158 BTU/lb-°F @Temperature 1830 °F |
|
Haynes HR-120® alloy, solution heat-treated aged at 1200°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Specific Heat Capacity | 0.660 J/g-°C @Temperature 900 °C |
0.158 BTU/lb-°F @Temperature 1650 °F |
|
Haynes HR-120® alloy, solution heat-treated aged at 1400°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Specific Heat Capacity | 0.663 J/g-°C @Temperature 1000 °C |
0.158 BTU/lb-°F @Temperature 1830 °F |
|
Haynes HR-120® alloy, solution heat-treated aged at 1400°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Specific Heat Capacity | 0.660 J/g-°C @Temperature 900 °C |
0.158 BTU/lb-°F @Temperature 1650 °F |
|
Haynes HR-120® alloy, solution heat-treated aged at 1600°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Specific Heat Capacity | 0.663 J/g-°C @Temperature 1000 °C |
0.158 BTU/lb-°F @Temperature 1830 °F |
|
Haynes HR-120® alloy, solution heat-treated aged at 1600°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Specific Heat Capacity | 0.660 J/g-°C @Temperature 900 °C |
0.158 BTU/lb-°F @Temperature 1650 °F |
|
Haynes HR-120® alloy, solution heat-treated aged at 1800°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Specific Heat Capacity | 0.663 J/g-°C @Temperature 1000 °C |
0.158 BTU/lb-°F @Temperature 1830 °F |
|
Haynes HR-120® alloy, solution heat-treated aged at 1800°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Specific Heat Capacity | 0.660 J/g-°C @Temperature 900 °C |
0.158 BTU/lb-°F @Temperature 1650 °F |
|
Haynes HR-120® alloy, solution heat-treated plate Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Specific Heat Capacity | 0.663 J/g-°C @Temperature 1000 °C |
0.158 BTU/lb-°F @Temperature 1830 °F |
|
Haynes HR-120® alloy, solution heat-treated plate Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Specific Heat Capacity | 0.660 J/g-°C | 0.158 BTU/lb-°F | |
Schott N-BASF2 Glass Information Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.660 J/g-°C | 0.158 BTU/lb-°F | |
Schott N-LASF45 Glass Information Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.660 J/g-°C | 0.158 BTU/lb-°F | |
Schott N-SF57 Glass Information Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.660 J/g-°C | 0.158 BTU/lb-°F | |
Schott N-SF57HT Glass Information Provided by SCHOTT North America, Inc. |