Specific Heat Capacity 0.149 J/g-°C
0.0356 BTU/lb-°F
CMW® THERMKON® 62 Tungsten Copper parts
For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc.