CMW® THERMKON® 62 Tungsten Copper parts

Category Metal , Metal Matrix Composite , Nonferrous Metal , Refractory Metal , Tungsten Alloy
Manufacturer CMW Inc.
Trade Name THERMKON®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CMW® THERMKON® 62 Tungsten Copper parts.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc.
Physical Properties Metric English Comments
Density 17.17 g/cc
0.6203 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 27
27
Tensile Strength, Ultimate 862 MPa
125000 psi
Tensile Strength, Yield 723 MPa
105000 psi
Modulus of Elasticity 255 GPa
37000 ksi
Flexural Modulus 1.24 GPa
180 ksi
Thermal Properties Metric English Comments
CTE, linear 6.10 µm/m-°C

@Temperature 20.0 °C
3.39 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 0.149 J/g-°C
0.0356 BTU/lb-°F
Thermal Conductivity 160 W/m-K
1110 BTU-in/hr-ft²-°F
Melting Point 1080 - 3410 °C
1980 - 6170 °F
Solidus 1080 °C
1980 °F
Liquidus 3410 °C
6170 °F
Component Elements Properties Metric English Comments
Copper, Cu 10 %
10 %
Tungsten, W 90 %
90 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000493 ohm-cm
0.00000493 ohm-cm
(35% IACS)