Polymer Property : Annealing Point = 815 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Annealing Point 435 °C
815 °F
Ferro EG 2992 Glaze and Sealant Glass
Glass Type: Bi-Zn-B Typical Powder Form: SRRG Typical Application: Ferrites Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and insu..
Annealing Point 435 °C
815 °F
Viscosity 10<sup>13</sup> dPa s; ISO 7884-4
Schott Glass 8095 Lead Glass
Lead glass (28% PbO), electrically highly insulating, highly x-ray absorbing General electrotechnical applicationInformation provided by SCHOTT AG.