Thermal Properties | Metric | English | Comments |
---|---|---|---|
Annealing Point | 435 °C | 815 °F | |
Ferro EG 2992 Glaze and Sealant Glass Glass Type: Bi-Zn-B Typical Powder Form: SRRG Typical Application: Ferrites Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and insu.. |
|||
Annealing Point | 435 °C | 815 °F | Viscosity 10<sup>13</sup> dPa s; ISO 7884-4 |
Schott Glass 8095 Lead Glass Lead glass (28% PbO), electrically highly insulating, highly x-ray absorbing General electrotechnical applicationInformation provided by SCHOTT AG. |