Thermal Properties | Metric | English | Comments |
---|---|---|---|
Annealing Point | 470 °C | 878 °F | |
Ferro IP 550 Thick Film Glass Glass Type: Pb-Si-B-Al Typical Powder Form: RWG Typical Application: General Ferro produces standard and custom glass products that are used in thick film compositions including resistors, conducto.. |
|||
Annealing Point | 470 °C | 878 °F | Viscosity 10<sup>13</sup> dPa s; ISO 7884-4 |
Schott Glass 8360 Lead-Free Soft Glass Soft glass, lead-free Encapsulation of semiconductor components at low temperature (diodes) The heavy metal content for the elements lead, mercury, cadmium, and hexavalent chromium is less than 10.. |
|||
Annealing Point | 470 °C | 878 °F | Viscosity 10<sup>13</sup> dPa s; ISO 7884-4 |
Schott Glass 8405 UV-transmitting Glass Sodium-potassium-barium-silicate glass, highly UV-transmitting Used as envelope for germicidal lamps (low-pressure mercury vapor discharge lamps) and for UV detectors The heavy metal content for t.. |