Schott Glass 8405 UV-transmitting Glass

Category Ceramic , Glass
Manufacturer Schott North America
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Schott Glass 8405 UV-transmitting Glass.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Sodium-potassium-barium-silicate glass, highly UV-transmitting Used as envelope for germicidal lamps (low-pressure mercury vapor discharge lamps) and for UV detectors The heavy metal content for the elements lead, mercury, cadmium, and hexavalent chromium is less than 100 ppm.Information provided by SCHOTT AG.
Physical Properties Metric English Comments
Density 2.51 g/cc

@Temperature 25.0 °C
0.0907 lb/in³

@Temperature 77.0 °F
Mechanical Properties Metric English Comments
Modulus of Elasticity 65.0 GPa
9430 ksi
Poissons Ratio 0.21
0.21
Thermal Properties Metric English Comments
CTE, linear 9.70 µm/m-°C

@Temperature 20.0 - 300 °C
5.39 µin/in-°F

@Temperature 68.0 - 572 °F
ISO 7991
Thermal Conductivity 1.00 W/m-K

@Temperature 90.0 °C
6.94 BTU-in/hr-ft²-°F

@Temperature 194 °F
Transformation Temperature, Tg 460 °C
860 °F
ISO 7884-8
Softening Point 665 °C
1230 °F
Viscosity 10<sup>7.6</sup> dPa s; ISO 7884-3
Working Point 1000 °C
1830 °F
Viscosity 10<sup>4</sup> dPa s; ISO 7884-2
Annealing Point 470 °C
878 °F
Viscosity 10<sup>13</sup> dPa s; ISO 7884-4
Optical Properties Metric English Comments
Refractive Index 1.505

@Wavelength 587.6 nm
1.505

@Wavelength 587.6 nm
UV Transmittance >= 75 %

@Thickness 1.00 mm,
Wavelength 253.7 nm
>= 75 %

@Thickness 0.0394 in,
Wavelength 253.7 nm
Electrical Properties Metric English Comments
Volume Resistivity 7.90e+6 ohm-cm

@Temperature 350 °C
7.90e+6 ohm-cm

@Temperature 662 °F
3.20e+8 ohm-cm

@Temperature 250 °C
3.20e+8 ohm-cm

@Temperature 482 °F
Dielectric Constant 6.5

@Frequency 1.00e+6 Hz,
Temperature 25.0 °C
6.5

@Frequency 1.00e+6 Hz,
Temperature 77.0 °F
Dielectric Loss Index 0.0045

@Frequency 1.00e+6 Hz,
Temperature 25.0 °C
0.0045

@Frequency 1.00e+6 Hz,
Temperature 77.0 °F
Chemical Properties Metric English Comments
Acid Class, SR 3
3
DIN 12116
Alkali Class, AR 2
2
ISO 695
Descriptive Properties Value Comments
Hydrolytic Resistance Class HGB 5
ISO 719
Stress-optical Coefficient K (10-6mm2N-1) 2.8
DIN 52314
tk100(°C) 280