Thermal Properties | Metric | English | Comments |
---|---|---|---|
Annealing Point | 570 °C | 1060 °F | |
Ferro CF 7574 Glaze and Sealant Glass Glass Type: Zn-B-Si Typical Powder Form: VSD Typical Application: Pyrex Silicon Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and .. |
|||
Annealing Point | 570 °C | 1060 °F | |
Ferro EG 2807 Metal Sealing Glass Type: Zn-B-Si (devit) Typical Powder Form: VSD Typical Application: Kovar Mo, W Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matc.. |
|||
Annealing Point | 570 °C | 1060 °F | Viscosity 10<sup>13</sup> dPa s; ISO 7884-4 |
Schott Glass 8326 Neutral Glass Tubing Neutral glass tubing, alkali resistance better as for DURAN® Special lab glass The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is less than 100 ppm.Info.. |