Ferro CF 7574 Glaze and Sealant Glass

Category Ceramic , Glass , Glaze
Manufacturer Ferro Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ferro CF 7574 Glaze and Sealant Glass.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Glass Type: Zn-B-Si Typical Powder Form: VSD Typical Application: Pyrex Silicon Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and insulating over glazes, binding agents and sealants for a variety of ceramic, metal, glass parts and substrates.Information provided by Ferro Corporation
Physical Properties Metric English Comments
Density 3.68 g/cc
0.133 lb/in³
Particle Size 20 µm
20 µm
50% of particles
<= 50 µm
<= 50 µm
Thermal Properties Metric English Comments
CTE, linear 3.40 µm/m-°C
1.89 µin/in-°F
at Set Pt.; Crystallized
4.40 µm/m-°C

@Temperature 260 °C
2.44 µin/in-°F

@Temperature 500 °F
Softening Point 644 °C
1190 °F
Annealing Point 570 °C
1060 °F
Transformation Temperature 555 °C
1030 °F
Processing Properties Metric English Comments
Processing Temperature 750 °C
1380 °F
Typical Firing Temperature