Polymer Property : Dropping Point = 90.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Dropping Point 90.0 - 105 °C
194 - 221 °F
Struktol PE(H)-100 Dispersion and Compounding Additive
Homopolymer, non-oxidized polyethylene wax.STRUKTOL® PE(H)-100 is a versatile polyethylene wax (homopolymer) used in natural and synthetic elastomers. It is used to improve flow and processabilit..