Polymer Property : Dropping Point = 105 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Dropping Point 76.0 - 105 °C
169 - 221 °F
Average value: 95.1 °C Grade Count:12
Overview of materials for Ethylene Acrylic Acid
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Acrylic Acid". Each property range of values reported is minimum and maximum values of appropri..
Dropping Point 90.0 - 105 °C
194 - 221 °F
Struktol PE(H)-100 Dispersion and Compounding Additive
Homopolymer, non-oxidized polyethylene wax.STRUKTOL® PE(H)-100 is a versatile polyethylene wax (homopolymer) used in natural and synthetic elastomers. It is used to improve flow and processabilit..
Dropping Point 95.0 - 105 °C
203 - 221 °F
Struktol TR 060 Blending Aid, Processing Additive
A mixture of light-colored aliphatic resins with a molecular weight below 2,000.At process temperatures, STRUKTOL® TR 060 melt has a natural tackiness and this "adhesive" nature enables it to act..