Thermal Properties | Metric | English | Comments |
---|---|---|---|
Dropping Point | 190 °C | 374 °F | ASTM D2265 |
ExxonMobil 0 Mobilux EP Mobilux EP 0, 1, 2, 3, and 023 products are a high performance family of five general-purpose industrial greases and two special-duty semi-fluid greases. These lithium hydroxystearate greases are fo.. |
|||
Dropping Point | 190 °C | 374 °F | ASTM D2265 |
ExxonMobil 1 Mobilux EP Mobilux EP 0, 1, 2, 3, and 023 products are a high performance family of five general-purpose industrial greases and two special-duty semi-fluid greases. These lithium hydroxystearate greases are fo.. |
|||
Dropping Point | 190 °C | 374 °F | ASTM D2265 |
ExxonMobil 3 Mobilux EP Mobilux EP 0, 1, 2, 3, and 023 products are a high performance family of five general-purpose industrial greases and two special-duty semi-fluid greases. These lithium hydroxystearate greases are fo.. |
|||
Dropping Point | 190 °C | 374 °F | ASTM D2265 |
ExxonMobil 2 Mobilux EP Mobilux EP 0, 1, 2, 3, and 023 products are a high performance family of five general-purpose industrial greases and two special-duty semi-fluid greases. These lithium hydroxystearate greases are fo.. |
|||
Dropping Point | 190 °C | 374 °F | |
Dow Corning MOLYKOTE® G 68 Semi-synthetic greaseInformation provided by Dow Corning |
|||
Dropping Point | >= 190 °C | >= 374 °F | |
Dow Corning MOLYKOTE® G-2001 Lithium thickened bearing grease based on synthetic hydrocarbonInformation provided by Dow Corning |
|||
Dropping Point | 190 °C | 374 °F | |
Dow Corning MOLYKOTE® LONGTERM 00 GREASE NLGI 00 mineral oil greaseInformation provided by Dow Corning |
|||
Dropping Point | >= 190 °C | >= 374 °F | |
Dow Corning MOLYKOTE® PG-75 GREASE Semi-Synthetic (Mineral/PAO) grease especially for vehicle track-rod jointsInformation provided by Dow Corning |
|||
Dropping Point | 190 °C | 374 °F | |
ChevronTexaco Block Grease Chevron Block Grease is a high melting point block grease.It is manufactured using highly refined base oils, a lithium thickener, and a special oxidation inhibitor which eliminates glazing and charr.. |
|||
Dropping Point | 190 °C | 374 °F | |
ChevronTexaco NLGI 2 Ultra Duty Grease EP FeaturesChevron Ultra-Duty Greases EP are versatile, multipurpose extreme pressure greases with high adhesive propertues designed for a wide variety of automotive and industrial applications.They ar.. |
|||
Dropping Point | 190 °C | 374 °F | ASTM D2265 |
ExxonMobil 0 Mobilux EP Mobilux EP 0, 1, 2, 3, and 023 products are a high performance family of five general-purpose industrial greases and two special-duty semi-fluid greases. These lithium hydroxystearate greases are fo.. |
|||
Dropping Point | 190 °C | 374 °F | ASTM D2265 |
ExxonMobil 1 Mobilux EP Mobilux EP 0, 1, 2, 3, and 023 products are a high performance family of five general-purpose industrial greases and two special-duty semi-fluid greases. These lithium hydroxystearate greases are fo.. |
|||
Dropping Point | 190 °C | 374 °F | ASTM D2265 |
ExxonMobil 2 Mobilux EP Mobilux EP 0, 1, 2, 3, and 023 products are a high performance family of five general-purpose industrial greases and two special-duty semi-fluid greases. These lithium hydroxystearate greases are fo.. |
|||
Dropping Point | 190 °C | 374 °F | ASTM D2265 |
ExxonMobil 3 Mobilux EP Mobilux EP 0, 1, 2, 3, and 023 products are a high performance family of five general-purpose industrial greases and two special-duty semi-fluid greases. These lithium hydroxystearate greases are fo.. |