ChevronTexaco Block Grease

Category Fluid , Lubricant , Lithium Gellant
Manufacturer ChevronTexaco Corp
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco Block Grease.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chevron Block Grease is a high melting point block grease.It is manufactured using highly refined base oils, a lithium thickener, and a special oxidation inhibitor which eliminates glazing and charring. It is fibrous-textured and dark brown in colorChevron Block Grease has good lubricant film retention and, thus, assures low starting torque and reduced friction during operation. Its uniform consistency and hardness throughout each block assures that the lubricant is fed evenly at a constant rate.Chevron Block Grease lubricates well in applications where operating temperatures up to 149°C are encountered. It is non corrosive to bronze bearings.ApplicationsChevron Block Grease is recommended for all bearings with open grease cellars, such as those on older kilns, rod and ball mills, laundry equipment, kiln cars, dehydrators, etc
Physical Properties Metric English Comments
Viscosity Measurement 62
62
Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 1427 SUS
1427 SUS
Saybolt Viscosity at 210°F 91 SUS
91 SUS
Kinematic Viscosity at 40°C (104°F) 265 cSt
265 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 17.5 cSt
17.5 cSt
ASTM D445
Mechanical Properties Metric English Comments
Penetration P(0), 1/10 mm 40
40
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 149 °C
300 °F
Minimum Service Temperature, Air 21.0 °C
69.8 °F
Flash Point 230 °C
446 °F
ASTM D92
Dropping Point 190 °C
374 °F
Descriptive Properties Value Comments
Color Dark Brown
Texture Fibrous
Thickener, % / type - / Lithium