Thermal Properties | Metric | English | Comments |
---|---|---|---|
Dropping Point | 288 °C | 550 °F | ASTM D2265 |
ExxonMobil Mobil Centaur Moly 1 Mobil Centaur Moly is a premium quality grease formulated with advanced calcium sulfonate thickener technology. The calcium sulfonate thickener in the Mobil Centaur Moly products represents a sign.. |
|||
Dropping Point | 288 °C | 550 °F | ASTM D2265 |
ExxonMobil Mobil 1 Synthetic Grease Mobil 1 Synthetic Grease is an NLGI No 2 high-performance grease which combines a synthetic base fluid with a lithium complex soap thickener. The thickener system provides a high dropping point, whi.. |
|||
Dropping Point | 288 °C | 550 °F | ASTM D2265 |
ExxonMobil Mobil Centaur Moly 1 Mobil Centaur Moly is a premium quality grease formulated with advanced calcium sulfonate thickener technology. The calcium sulfonate thickener in the Mobil Centaur Moly products represents a sign.. |
|||
Dropping Point | 288 °C | 550 °F | |
ConocoPhillips 1 HD Calcium Grease NLGI No. 1 Description: Conoco HD Calcium Grease is a formulated product, ideally suited for equipment exposed to corrosive fluids, saltwater or extremely high temperatures. HD Calcium Grease is used exclusive.. |
|||
Dropping Point | 288 °C | 550 °F | |
ConocoPhillips 2 HD Calcium Grease NLGI No. 2 Description: Conoco HD Calcium Grease is a formulated product, ideally suited for equipment exposed to corrosive fluids, saltwater or extremely high temperatures. HD Calcium Grease is used exclusive.. |
|||
Dropping Point | 288 °C | 550 °F | ASTM D2265 |
ExxonMobil Mobil 1 Synthetic Grease Mobil 1 Synthetic Grease is an NLGI No 2 high-performance grease which combines a synthetic base fluid with a lithium complex soap thickener. The thickener system provides a high dropping point, whi.. |
|||
Dropping Point | >= 288 °C | >= 550 °F | ASTM D566, ISO2176 |
Chesterton 783 ACR Anti-Seize Compound Description: Chesterton® 783 ACR represents the newest generation of anti-seize compound. A proprietary blend of ultra-fine inorganic solid lubricants, 783 ACR can be used under extremely severe co.. |
|||
Dropping Point | 288 °C | 550 °F | ASTM D2265, DIN 51 801/1 |
Chesterton 633 SXCM Synthetic, Extreme Pressure & Corrosion Resistant Grease-with Moly Description: Chesterton® 633 Synthetic Extreme Pressure & Corrosion Resistant Grease with Moly is the one grease to use for the most demanding lubricating needs. It is a multi-purpose workhorse wit.. |