Thermal Properties | Metric | English | Comments |
---|---|---|---|
Dropping Point | 287 °C | 549 °F | |
ChevronTexaco FM NLGI 2 Grease EP FeaturesChevron FM Greases EP are high performance, multipurpose food machinery greases that are white in color, odorless, tasteless, and water-resistant. Available in three grades, Chevron FM Greas.. |
|||
Dropping Point | 287 °C | 549 °F | |
ChevronTexaco Cygnus® Grease NLGI Grade 2 Texaco Cyngus Greases are high performance, multipurpose food machinery greases that are white in color, odorless, tasteless, and water-resistant. Available in two grades, Texaco Cyngnus Greases wer.. |