Thermal Properties Metric English Comments
Dropping Point 122 - 128 °C
252 - 262 °F
Struktol TPW 012 Processing Additive
An optimized blend of special waxes and oleo chemicals.STRUKTOL® TPW 012 is a formulated blend of lubricants designed to provide optimum processing, surface and physical property characteristics ..