Thermal Properties | Metric | English | Comments |
---|---|---|---|
Dropping Point | 215 °C | 419 °F | ASTM D2265 |
ExxonMobil Mobilgrease XTC Mobilgrease XTC is an extra high performance product designed for use in high speed coupling applications. It is manufactured with a selected high viscosity mineral base oil and an extremely effecti.. |
|||
Dropping Point | 215 °C | 419 °F | |
ChevronTexaco Coupling Grease FeaturesChevron Coupling Grease is a brown, stringy and tacky grease manufactured using a high viscosity base oil, a lithium soap thickener, rust and oxidation inhibitors, and extreme pressure and p.. |
|||
Dropping Point | 215 °C | 419 °F | |
ChevronTexaco Coupling Grease NLGI Grade 0/1 Texaco Coupling Grease delivers value through:Superior film strength — Formulated with a high viscosity base oil and polymer for superior film strengthLittle to no oil separation in high-speed coup.. |
|||
Dropping Point | 215 °C | 419 °F | ASTM D2265 |
ExxonMobil Mobilgrease XTC Mobilgrease XTC is an extra high performance product designed for use in high speed coupling applications. It is manufactured with a selected high viscosity mineral base oil and an extremely effecti.. |