Material Notes:
Texaco Coupling Grease delivers value through:Superior film strength — Formulated with a high viscosity base oil and polymer for superior film strengthLittle to no oil separation in high-speed couplings under high centrifugal forcesExcellent adhesion — Stringy and tackyReduced leakage because of a tackiness polymer additiveExtreme pressure, rust, and oxidation protectionExtended relubrication intervals — Avoids costly maintenance and downtimeExcellent low temperature pumpability down to 0°C (32°F)Texaco Coupling Grease is a brown, stringy, tacky grease manufactured using a high viscosity base oil, a lithium soap thickener, rust and oxidation inhibitors, and extreme pressure and polymer tackiness additives.It is designed for all high-speed grease lubricated flexible couplings and is specially formulated to provide specific resistance to centrifugal separation in highspeed gear or grid couplings.Texaco Coupling Grease has high load-carrying capacity and therefore provides good protection of lubricated parts against wear.Texaco Coupling Grease is specifically designed for the lubrication of high-speed grease lubricated flexible couplings where high centrifugal forces are present.It is recommended for use in high-speed grid, gear, or chain couplings in a variety of industrial applications.Texaco Coupling Grease meets the coupling requirements of AGMA CG-1 and CG-2 type couplings.Texaco Coupling Grease exhibits little to no oil separation in the ASTM D 4425 high-speed centrifuge test.Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.Notes:Minimum operating temperature is the lowest temperature at which a grease, already in place, could be expected to provide lubrication. Most greases cannot be pumped at these minimum temperatures.Maximum operating temperature is the highest temperature at which the grease could be used with frequent (daily) relubrication.Determined on mineral oil extracted by vacuum filtration.CPS Number: 221912; MSDS Number: 8803
Physical Properties Metric English Comments
Kinematic Viscosity at 100°C (212°F) 250 cSt
250 cSt
See Note 3.
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 400 kg
882 lb (mass)
Penetration P(0), 1/10 mm 252
252
Unworked, 25°C (77°F)
Penetration P(60), 1/10 mm 336
336
Unknown Amount of Work, 25°C (77°F)
Oil Separation <= 2.0 %
<= 2.0 %
Centrifugal, 24 h
Timken Test 18100 g
40.0 lb
OK Load
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 162 °C
324 °F
See Note 2.
Minimum Service Temperature, Air -29.0 °C
-20.2 °F
See Note 1.
Dropping Point 215 °C
419 °F
Descriptive Properties Value Comments
Color Dark Brown
Texture Smooth, Tacky
Thickener, % 5
Lithium/Polymer
Copyright © lookpolymers.com All Rights Reserved