Polymer Property : Dropping Point = 205 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Dropping Point 96.0 - 108 °C
205 - 226 °F
Struktol TR 016 Processing Additive
A blend of fatty acid metal soap and an amideThe amide of STRUKTOL® TR 016 has sites available for hydrogen bonding, and is therefore able to act as a physical coupling agent between polymer syst..