Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Struktol TR 016 Processing Additive

Category Other Engineering Material , Additive/Filler for Polymer , Polymer
Manufacturer Struktol
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Struktol TR 016 Processing Additive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A blend of fatty acid metal soap and an amideThe amide of STRUKTOL® TR 016 has sites available for hydrogen bonding, and is therefore able to act as a physical coupling agent between polymer systems and a range of filler materials. This permits STRUKTOL® TR 016 to act as an efficient blending or dispersing agent in highly filled systems, providing a more uniform and homogenous initial mix. At processing conditions, STRUKTOL® TR 016 is an effective internal lubricant for the polyolefins, PVC, PS, ABS and many of the TPO systems. Application areas recommended for STRUKTOL® TR 016 in highly-filled systems include TPEs and TPO compounds, filled olefins, flame retarded polymers and color concentrate materials. In addition, STRUKTOL® TR 016 can be useful in those standard unfilled polymers where reduced viscosity and improved flow are desirable at processing conditions. In many systems, better surface appearance and lower and more uniform mold shrinkage will be seen. Physical property losses are quite small for most compounds at normal addition levels of STRUKTOL® TR 016. Benefits of STRUKTOL® TR 016 include: Improved flow at processing temperatures Better surface appearance Easier mold release in many systemsBetter dispersion of fillers and additivesNon-blooming propertiesFDA Status: 173.340; 175.105; 175.300; 175.320; 176.170; 176.200; 176.210; 177.1200; 177.2260; 177.2410; 177.2600; 177.2010; 178.2010; 178.3860; 181.29; 184.1229
Physical Properties Metric English Comments
Specific Gravity 0.980 g/cc
0.980 g/cc
Additive Loading 0.25 - 1.0 %
0.25 - 1.0 %
Thermal Properties Metric English Comments
Dropping Point 96.0 - 108 °C
205 - 226 °F
Processing Properties Metric English Comments
Shelf Life >= 24.0 Month
>= 24.0 Month
Descriptive Properties Value Comments
Appearance Pale beads or pastilles
Users viewing this material also viewed the following: