Polymer Property : Dropping Point = 180 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Dropping Point 180 °C
356 °F
ASTM D2265
ExxonMobil 111 Mobilux EP
Mobilux EP 111 is an extra high performance grease primarily designed for lubrication of all designs of couplings. It is specifically formulated to resist centrifugal separation of the oil from the ..
Dropping Point 180 °C
356 °F
ASTM D2265
ExxonMobil 111 Mobilux EP
Mobilux EP 111 is an extra high performance grease primarily designed for lubrication of all designs of couplings. It is specifically formulated to resist centrifugal separation of the oil from the ..