Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 36.0 °C | 96.8 °F | |
LG Chemical LC565 Polyolefin Elastomer for Polymer Modification Features: Improved impact strength in polypropylene; Excellent filler acceptance; Available as pellet form; Outstanding toughness with flexible performance; and Reduction of product weightApplicatio.. |
|||
Melting Point | 36.0 °C | 96.8 °F | DSC, 10°C/min (peak); DuPont Test |
Dow Engage® ENR 7467.00 Ethylene-Butene Copolymer Description: ENR 7467.00 is a high performance ethylene-butene copolymer, offering superior impact properties for more demanding TPO applications. The polymer has very low crystallinity and is avail.. |
|||
Melting Point | 36.0 °C | 96.8 °F | |
BASF Ethylene Carbonate S Formula: C3H4O3CAS: 96-49-1Description: Ethylene carbonate is a colorless to yellow solid, with a fruity odor. It is fully soluble in water.Synonyms: EC, 1,3-Dioxolan-2-oneApplications: Intermediat.. |
|||
Melting Point | 36.0 °C | 96.8 °F | |
BASF PolyTHF® 2000 Polyether Description: PolyTHF 2000 is a colorless, odorless waxy substance. It is sparingly soluble in water and soluble organic solvents.Applications: Intermediate used in the production of: Synthesis of el.. |
|||
Melting Point | 36.0 - 42.0 °C | 96.8 - 108 °F | |
BASF 2,4-Ethylmethylimidazole S Formula: C6H10O2CAS: 931-36-2Description: 2,4-Ethylmethylimidazole S is a colorless to yellowish liquid with an amine-like odor.Synonyms: EMI, 2-Ethyl-4-methylimidazole, 4-Methyl-2-ethylimidazole, 2.. |