Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 40.0 - 42.0 °C | 104 - 108 °F | |
BASF HDO® 1,6-Hexanediol Flakes Formula: C6H14O2CAS: 629-11-8Description: 1,6-Hexanediol (HDO) flakes are a colorless, odorless solids or molten masses. It is miscible in water in all proportions and soluble in ethanol.Synonyms: .. |
|||
Melting Point | 40.0 - 42.0 °C | 104 - 108 °F | |
BASF HDO® 1,6-Hexanediol Molten Formula: C6H14O2CAS: 629-11-8Description: 1,6-Hexanediol Molten (HDO) is a colorless, odorless molten mass or solid. It is miscible in water in all proportions and soluble in ethanol.Synonyms: Hexa.. |
|||
Melting Point | 36.0 - 42.0 °C | 96.8 - 108 °F | |
BASF 2,4-Ethylmethylimidazole S Formula: C6H10O2CAS: 931-36-2Description: 2,4-Ethylmethylimidazole S is a colorless to yellowish liquid with an amine-like odor.Synonyms: EMI, 2-Ethyl-4-methylimidazole, 4-Methyl-2-ethylimidazole, 2.. |