Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 870 - 920 °C | 1600 - 1690 °F | |
Wieland 1403 Wilaform Gold Hard yellow gold alloy. Universally applicable in decoration production. Since it does not posses a very fine-grained structure it is used frequently for chainsApplications: casting, chains, lamin.. |