Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 79.0 - 89.0 °C | 174 - 192 °F | |
Fine Organics FINALUX G1 Lubricant Additive Applications:Lubricant for:rigid PVC pipesconduitsfittingscable compoundsInformation provided by Fine Organics |
|||
Melting Point | 80.0 - 89.0 °C | 176 - 192 °F | |
Indium Corp. Indalloy 31 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 80.0 - 89.0 °C | 176 - 192 °F | |
Indium Corp. Indalloy 32 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 76.0 - 89.0 °C | 169 - 192 °F | |
Solvay RHODAFAC® ASI-100 Octyl phosphonic acid Identification: ALKYL PHOSPHONATE DERIVATIVECAS: 4724 – 48 – 5EINECS: 225 – 218 – 5Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: Corrosion inhi.. |
|||
Melting Point | 51.0 - 89.0 °C | 124 - 192 °F | ASTM D3418(DSC) |
DuPont Surlyn® 9945 Thermoplastic Ionomer Resin Surlyn® 9945 provides high flow properties and consistent, easy processing behavior in molded and extruded applications. It is positioned in the medium/high acid, high neutralization area of the i.. |