Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 80.0 °C | 176 °F | Freezing point via DSC/ASTM D3418 |
DuPont Bynel® 3048 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
(discontinued **) Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Melting Point | 80.0 - 155 °C | 176 - 311 °F | Average value: 120 °C Grade Count:6 |
Overview of materials for Cyclo Olefin Polymer This property data is a summary of similar materials in the MatWeb database for the category "Cyclo Olefin Polymer". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Melting Point | 80.0 - 110 °C | 176 - 230 °F | TMA Melt Range |
Huntsman IROGRAN® CA116-203 TPU-Polyester Introduction: IROGRAN CA116-203 is a high performance polyester based thermoplastic polyurethane intended for flat die extrusion applications. IROGRAN CA116-203 is part of the HUNTSMAN film and shee.. |
|||
Melting Point | 80.0 - 110 °C | 176 - 230 °F | TMA Melt Range |
Huntsman IROGRAN® CA116-205 TPU-Polyester Introduction: IROGRAN CA116-205 is a high performance polyester based thermoplastic polyurethane intended for flat die extrusion applications. IROGRAN CA116-205 is part of the HUNTSMAN film and shee.. |
|||
Melting Point | 80.0 - 88.0 °C | 176 - 190 °F | |
M Chemical GUARD DOGâ„¢ UV328 Benzotriazole UV Absorber GUARD DOGâ„¢ UV328 light stabilizer is a derivative of Benzotriazole that has exceptionally strong and broad-range UV absorption properties throughout the UV spectrum specially designed for polym.. |
|||
Melting Point | 80.0 - 86.0 °C | 176 - 187 °F | |
M Chemical GUARD DOGâ„¢ UV770 HALS Light Stabilizer GUARD DOGâ„¢ UV770 unhindered amine light stabilizer is a highly effective radical scavenger that protects polymers against degradation caused by exposure to UV radiation.Applications: Extremely.. |
|||
Melting Point | 80.0 - 89.0 °C | 176 - 192 °F | |
Indium Corp. Indalloy 31 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 80.0 °C | 176 °F | TMA; MCI Method |
Mitsui APELâ„¢ APL8008T Cyclo Olefin Copolymer (COC) This material possesses many characteristics inherent in polyolefins such as excellent electrical insulating properties and outstanding moisture resistance. In addition, it features good melt proces.. |
|||
Melting Point | 80.0 - 84.0 °C | 176 - 183 °F | MQSA 70 A |
Lubrizol Advanced Materials Pearlbond® ECO D590 Thermoplastic Polyurethane Pearlbond™ ECO D590 is a linear, aromatic bio-polyurethane based on specialty polyol from renewable sources, supplied in form of white spherical granules, with an extremely high crystallization.. |
|||
Melting Point | 80.0 - 85.0 °C | 176 - 185 °F | MQSA 70 A |
Lubrizol Advanced Materials Pearlbond® Eco D900 Thermoplastic Polyurethane Pearlbond™ ECO D900 is a linear, aromatic polyurethane based on specialty polyol from renewable sources. It contains 67% of renewable material as certified according to ASTM-D6866. It is suppli.. |
|||
Melting Point | 80.0 °C | 176 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Nucrel® 31001 Ethylene-Acrylic Acid Copolymer Resin for Blown and Cast Film 9.5 wt% Acrylic Acid.Nucrel® 31001 is an ethylene-acrylic acid copolymer resin available for use in blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins.F.. |
|||
Melting Point | 80.0 - 94.0 °C | 176 - 201 °F | ASTM D3418(DSC) |
DuPont Nucrel® 699 Ethylene-Methacrylic Acid Copolymer Resin Nucrel® 599 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Melting Point | 80.0 °C | 176 °F | Freezing Point, DSC; ASTM D3418 |
DuPont Nucrel® AE High Performance Adhesive and Sealant Resin Nucrel® Nucrel® AE is a terpolymer of ethylene, methacrylic acid, and acrylate, available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment designe.. |
|||
Melting Point | 80.0 °C | 176 °F | Exxon Method |
ExxonMobil Optema® TC-110 Cast Ethylene Methyl Acrylate Product Description: Optema TC 110 is an ethylene methyl acrylate copolymer specifically formulated to offer extrusion and property performance for blown and cast film applications. It can produce f.. |
|||
Melting Point | 80.0 °C | 176 °F | DSC |
Arkema Group LOTRYL® 20 MA 08 Copolymer Ethylene - Methyl Acrylate LOTRYL® 20 MA 08 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the high methyl acrylate content, LOTRYL® 20 MA 08 is a polyme.. |
|||
Melting Point | 80.0 °C | 176 °F | DSC |
Arkema Group LOTRYL® 28 BA 175 Copolymer Ethylene - Butyl Acrylate LOTRYL® 28 BA 175 is a random copolymer of ethylene and butyl acrylate, prepared by the high pressure polymerization process. Co-monomer content is 28% in weight. LOTRYL® 28 BA 175 is particularly.. |
|||
Melting Point | 80.0 °C | 176 °F | D.S.C. method |
Arkema Group Orevac® 18216 Maleic Anhydride modified EVA Orevac® 18216 resin is a maleic anhydride modified ethylene - vinyl acetate copolymer designed for the coextrusion of multilayer barrier structures providing outstanding adhesion between layers.Inf.. |
|||
Melting Point | 80.0 °C | 176 °F | DSC |
Arkema Group OREVAC® 9304 EVA Terpolymer OREVAC® is a range of ethylene-vinyl acetate copolymers modified by adjunction of polar groups which, when molten, have excellent adhesive properties to various substrates. They are supplied as fre.. |
|||
Melting Point | 80.0 °C | 176 °F | |
C.O.I.M. UREXTER® F 3 Polyurethane Two-Component Compound Description: Polyester PU System for shoe sole manufacturingInformation provided by P.A.T. Products, Inc. |
|||
Melting Point | 80.0 °C | 176 °F | |
C.O.I.M. UREXTER® Lp 2500_30 Polyurethane Two-Component Compound Description: Polyester PU System for shoe sole manufacturingInformation provided by P.A.T. Products, Inc. |
|||
Melting Point | 80.0 °C | 176 °F | |
C.O.I.M. UREXTER® Lp 285 Polyurethane Two-Component Compound Description: Polyester PU System for shoe sole manufacturingInformation provided by P.A.T. Products, Inc. |
|||
Melting Point | 80.0 °C | 176 °F | |
C.O.I.M. UREXTER® T 404 Polyurethane Two-Component Compound Description: Polyester PU System for shoe sole manufacturingInformation provided by P.A.T. Products, Inc. |
|||
Melting Point | 80.0 °C | 176 °F | DSC |
Arkema Group LOTADER® 4503 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 4503 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high-pressure autoclave process.LOTADER 4503 is a versatile adhesive for extrusion lamination, des.. |
|||
Melting Point | 80.0 °C | 176 °F | DSC |
Arkema Group LOTADER® 5500 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 5500 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high pressure autoclave process. These grade is characterised by a high fluidity. Functional group.. |
|||
Melting Point | 80.0 °C | 176 °F | DSC |
Arkema Group EVATANE® 24-03 Copolymer Ethylene - Vinyl Acetate EVATANE® 24-03 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 24-03 is stabilized with antioxidants. The High Vinyl Acetate co.. |
|||
Melting Point | 80.0 °C | 176 °F | |
M. Holland Company MAGMA® LM311-D LLDPE
(discontinued **) Features: Good Processability, Good Puncture Resistance, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland. |
|||
Melting Point | >= 80.0 °C | >= 176 °F | AM6512 |
Solvay RHODAPHOSE® TRIPHENYL PHOSPHINE Phosphorus Derivative Identification: TRIPHENYLPHOSPHINECAS: 603 – 35 – 0Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: TRIPHENYL PHOSPHINE is an intermediate for use as a phase transf.. |