Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 56.0 - 83.0 °C | 133 - 181 °F | ASTM D3418(DSC) |
DuPont Nucrel® 2906 Ethylene-Methacrylic Acid Copolymer Resin
(discontinued **) Nucrel® 2906 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for.. |
|||
Melting Point | 55.0 - 83.0 °C | 131 - 181 °F | ASTM D3418(DSC) |
DuPont Nucrel® 2940 Ethylene-Methacrylic Acid Copolymer Resin
(discontinued **) Nucrel® 2940is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Melting Point | 81.0 - 83.0 °C | 178 - 181 °F | |
Hong Kun Group UV 328 UV Absorber UV328 is a strong ultraviolet light absorber in the 290-400nm region. It provides effective light stabilization and prevents the yellowing and degradation of polymers such as PVC, unsaturated polyes.. |