Thermal Properties Metric English Comments
Melting Point 56.0 - 83.0 °C
133 - 181 °F
ASTM D3418(DSC)
DuPont Nucrel® 2906 Ethylene-Methacrylic Acid Copolymer Resin  (discontinued **)
Nucrel® 2906 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for..
Melting Point 56.0 °C
133 °F
Dow Method
Dow AFFINITY™ EG 8150G Ethylene alpha-olefin copolymer
AFFINITY™ EG 8150G Polyolefin Plastomer (POP) is produced via INSITE™ Technology. It is a general purpose ethylene alpha-olefin copolymer exhibiting high flexibility and elasticity. It can be ut..