Polymer Property : Melting Point = 788 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 788 °C
1450 °F
Heatbath/Park Sta-Hard 45 High Speed Hardening Salt
A stable salt for neutral heating of ferrous and nonferrous alloys. Sta-Hard45 is similar to Sta-Hard 17, but provides higher working temperatures.Information provided by Heatbath Corporation - Park..
Melting Point 788 °C
1450 °F
Heatbath/Park Sta-Hard 45 Neutral Salt
A stable salt for neutral heating of ferrous and nonferrous alloys. Sta-Hard45 is similar to Sta-Hard 17, but provides higher working temperatures.Information provided by Heatbath Corporation - Park..
Melting Point 788 °C
1450 °F
Heatbath/Park Sta-Hard 45 Steel Brazing Neutral Salt
A higher temperature range neutral salt used for brass or copper brazing.Information provided by Heatbath Corporation - Park Metallurgical.