Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 788 °C | 1450 °F | |
Heatbath/Park Sta-Hard 45 High Speed Hardening Salt A stable salt for neutral heating of ferrous and nonferrous alloys. Sta-Hard45 is similar to Sta-Hard 17, but provides higher working temperatures.Information provided by Heatbath Corporation - Park.. |
|||
Melting Point | 788 °C | 1450 °F | |
Heatbath/Park Sta-Hard 45 Neutral Salt A stable salt for neutral heating of ferrous and nonferrous alloys. Sta-Hard45 is similar to Sta-Hard 17, but provides higher working temperatures.Information provided by Heatbath Corporation - Park.. |
|||
Melting Point | 788 °C | 1450 °F | |
Heatbath/Park Sta-Hard 45 Steel Brazing Neutral Salt A higher temperature range neutral salt used for brass or copper brazing.Information provided by Heatbath Corporation - Park Metallurgical. |
|||
Melting Point | 790 °C | 1450 °F | |
Solvay Chemicals Lithium Cryolite Lithium Cryolite (Li3AlF6) is used for the production of abrasives, welding agents and soldering agents. Trilithium hexafluoroaluminate: CAS-No.: 13821-20-0 / EC-No.: 237-509-4Uses: Welding and sold.. |