Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 24.0 °C | 75.2 °F | ASTM D2117 |
Lushan EF-3 Adhesive Resin for Coextruded Multi-layer Barrier Packaging Film Adhesive resin Lushan series for multi-layer barrier food packaging film has durable bonding properties when adheres to Polarity materials, such as PE, PP and PA, EVOH, etc. Adhesive resin Lushan se.. |
|||
Melting Point | 24.0 - 26.0 °C | 75.2 - 78.8 °F | |
Solvay Chemicals Chlorodifluoroacetic acid CAS-No.: 76-04-0 / EC-No.: 200-928-8 Uses: Chemical intermediateInformation provided by Solvay |