Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melting Point = 24.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 24.0 °C
75.2 °F
ASTM D2117
Lushan EF-3 Adhesive Resin for Coextruded Multi-layer Barrier Packaging Film
Adhesive resin Lushan series for multi-layer barrier food packaging film has durable bonding properties when adheres to Polarity materials, such as PE, PP and PA, EVOH, etc. Adhesive resin Lushan se..
Melting Point 24.0 - 26.0 °C
75.2 - 78.8 °F
Solvay Chemicals Chlorodifluoroacetic acid
CAS-No.: 76-04-0 / EC-No.: 200-928-8 Uses: Chemical intermediateInformation provided by Solvay
Copyright © lookpolymers.com All Rights Reserved