Polymer Property : Melting Point = 7020 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 3880 °C
7020 °F
Momentive Performance Materials Tantalum Carbide (TaC) Coating
High temperature protective coating for graphite.TaC, NbC, and ZrC coatings resist chemical attack by corrosive liquids and gases at very high temperatures. They are finding increasing acceptance i..
Melting Point 3880 °C
7020 °F
Acerde Tantalum Carbide
Tantalum Carbide key properties: Extremely hard refractory ceramic material. The hardness is only exceeded by diamond, Very High melting point, High DensityTantalum Carbide main applications domains..