Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 48.0 - 58.0 °C | 118 - 136 °F | |
Fine Organics FINALUX G 601 Lubricant Additive Applications: Universal internal lubricant for rigid PVC and foamed PVC, applicable independently of stabilizing system. Pseudo-plasticizer for PVC. Low improver and lubricant for PMMAInformation .. |