Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 48.0 °C | 118 °F | |
DuPont Fusabond® MN493D Ethylene Octene Copolymer
(discontinued **) Typical Use: Nylon 6 toughenerNylon 6/6 toughenerComplies to FDA 21CFR 175.105Availability: North AmericaInformation provided by DuPont. |
|||
Melting Point | 48.0 °C | 118 °F | |
DuPont Fusabond® MN494D Ethylene Octene Copolymer
(discontinued **) Typical Use: Nylon 6 toughenerNylon 6/6 toughenerAvailability: North AmericaInformation provided by DuPont. |
|||
Melting Point | 48.0 - 112 °C | 118 - 234 °F | Average value: 75.6 °C Grade Count:70 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade". Each property range of values reported .. |
|||
Melting Point | 48.0 - 58.0 °C | 118 - 136 °F | |
Fine Organics FINALUX G 601 Lubricant Additive Applications: Universal internal lubricant for rigid PVC and foamed PVC, applicable independently of stabilizing system. Pseudo-plasticizer for PVC. Low improver and lubricant for PMMAInformation .. |
|||
Melting Point | >= 48.0 °C | >= 118 °F | |
Solvay AG-RHOâ„¢ DS 440 A Surfactant Description: Nonionic Surfactant blend to be used as a wetting agent for glyphosate adjuvants.Chemical Name: NONIONIC SURFACTANT BLENDSolubility: WaterAvailable in: Asia Pacific, Europe, Latin Ameri.. |
|||
Melting Point | 48.0 °C | 118 °F | |
Solvay SOPROPHOR® S/40 FLAKES Surfactant Description: Multipurpose dispersing agent for SC formulationsIdentification: ETHOXYLATED POLYARYLPHENOLSolubility: Soluble in water and most polar and aromatic solvents.Available in: Asia Pacific, .. |
|||
Melting Point | 48.0 °C | 118 °F | Freezing point via DSC/ASTM D3418 |
DuPont Bynel® E418 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin Bynel® Series 3800 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Melting Point | 48.0 °C | 118 °F | Freezing Point; ASTM D3417 |
DuPont Elvax® 3182-2 Ethylene Vinyl Acetate DuPont™ Elvax® 3182-2 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. Applicat.. |
|||
Melting Point | 48.0 °C | 118 °F | DSC, 10°C/min (peak); DuPont Test |
Dow Engage® ENR 7380.00 Ethylene-Butene Copolymer Description: ENR 7380.00 is a revolutionary new ethylene-butene copolymer with higher molecular weight, better toughness, and higher melt strength than other commercially available polyolefin elasto.. |
|||
Melting Point | 48.0 °C | 118 °F | DSC |
Arkema Group EVATANE® 42-60 Copolymer Ethylene - Vinyl Acetate EVATANE 42-60 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE 42-60 is stabilized with antioxidants and contains slip and antibloc.. |
|||
Melting Point | 48.0 °C | 118 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Elvax® 3175LG Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion
(discontinued **) 28 wt% Vinyl Acetate.Elvax® 3175 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.. |
|||
Melting Point | 48.0 °C | 118 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Elvax® 3175 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion 28 wt% Vinyl Acetate.Elvax® 3175 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.. |