Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 565 - 572 °C | 1050 - 1060 °F | in contact with aluminium |
Solvay Chemicals NOCOLOK® CB Flux Potassium Silicofluoride Reactive flux for brazing of aluminumCAS-No.: 16871-90-2 Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration and Household & Electrical AppliancesInformation provided .. |
|||
Melting Point | 565 - 572 °C | 1050 - 1060 °F | |
Solvay Chemicals NOCOLOK® Flux Drystatic Potassium Fluoroaluminate Flux using electrostatic/dry powder coating. Classifications: HS No.: 38109090 /CAS-No.: 60304-36-1Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration and Household & .. |
|||
Melting Point | 565 - 572 °C | 1050 - 1060 °F | |
Solvay Chemicals NOCOLOK® Flux P2 Potassium Fluoroaluminate Mixtures of NOCOLOK® Flux P2 with NOCOLOK® Flux allow for gradual viscosity adjustments in suspensions to suit specific process conditions.HS No.: 38109090 /CAS-No.: 60304-36-1Uses: Automoti.. |
|||
Melting Point | 565 - 572 °C | 1050 - 1060 °F | (Addition of CsAIF4 will reduce melting point) |
Solvay Chemicals NOCOLOK® Ultra Flux Paste A flux paste specifically formulated for providing a viscous homogeneous mixture of NOCOLOK® Flux (35–50%) in an organic carrier for brazing aluminum cladded interfaces where traditional wat.. |
|||
Melting Point | 565 - 575 °C | 1050 - 1070 °F | in contact with Al/Si filter metal |
Solvay Chemicals NOCOLOK® Zn Flux Reactive flux alternative to arc spray Zn coating.HS No.: 38109090 /CAS-No.: 13827-02-6Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration and Household & Electrical .. |