Polymer Property : Melting Point = 1060 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 565 - 572 °C
1050 - 1060 °F
in contact with aluminium
Solvay Chemicals NOCOLOK® CB Flux Potassium Silicofluoride
Reactive flux for brazing of aluminumCAS-No.: 16871-90-2 Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration and Household & Electrical AppliancesInformation provided ..
Melting Point 565 - 572 °C
1050 - 1060 °F
Solvay Chemicals NOCOLOK® Flux Drystatic Potassium Fluoroaluminate
Flux using electrostatic/dry powder coating. Classifications: HS No.: 38109090 /CAS-No.: 60304-36-1Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration and Household & ..
Melting Point 565 - 572 °C
1050 - 1060 °F
Solvay Chemicals NOCOLOK® Flux P2 Potassium Fluoroaluminate
Mixtures of NOCOLOK® Flux P2 with NOCOLOK® Flux allow for gradual viscosity adjustments in suspensions to suit specific process conditions.HS No.: 38109090 /CAS-No.: 60304-36-1Uses: Automoti..
Melting Point 564 - 572 °C
1050 - 1060 °F
Solvay Chemicals NOCOLOK® Flux Potassium Fluoroaluminate
A high quality fluxing agent for brazing aluminum components. Classifications: HS No.: 38109090/CAS-No.: 60304-36-1Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration ..
Melting Point 564 - 572 °C
1050 - 1060 °F
NOCOLOK Flux
Solvay Chemicals NOCOLOK® Sil Flux (fine grade)
Reactive flux for brazing of aluminum and filler alloy generating flux for brazing aluminum. Classifications: HS No.: 38109090 /CAS-No.: 60304-36-1Composition: either 2:1: 66.6 % ± 1.5 % -NOCOLOK..
Melting Point 565 - 572 °C
1050 - 1060 °F
(Addition of CsAIF4 will reduce melting point)
Solvay Chemicals NOCOLOK® Ultra Flux Paste
A flux paste specifically formulated for providing a viscous homogeneous mixture of NOCOLOK® Flux (35–50%) in an organic carrier for brazing aluminum cladded interfaces where traditional wat..
Melting Point 564 - 572 °C
1050 - 1060 °F
NOCOLOK Flux
Solvay Chemicals NOCOLOK® Sil Flux (extra fine grade)
Reactive flux for brazing of aluminum and filler alloy generating flux for brazing aluminum Classifications: HS No.: 38109090 /CAS-No.: 60304-36-1Composition: either 2:1: 66.6 % ± 1.5 % -NOCOLOK ..