Melting Point | 53.0 - 63.0 °C | 127 - 145 °F | |
Fine Organics FINALUX G 200 Lubricant Additive Applications: External lubricant for rigid and soft PVCInformation provided by Fine Organics |
|||
Melting Point | 53.0 °C | 127 °F | Freezing Point; ASTM D3418, ISO 3146 |
DuPont™ Elvax® 3175LGA Ethylene Vinyl Acetate DuPont™ Elvax® 3175LGA is an extrudable ethylene-vinyl acetate copolymer resin containing low gel material available in pellet form for use in conventional extrusion equipment designed to process .. |
|||
Melting Point | 53.0 °C | 127 °F | ASTM D3418 |
E-Polymers EFLEX® M100 Ethylene Octene Copolymer M-series: E-FLEX M series resins are a maleic anhydride grafted (MAH) polymer concentrate designed as synthetic rubber and polyolefin manufactured by E-Polymers. It offers excellent adhesion to nyl.. |
|||
Melting Point | 53.0 °C | 127 °F | ASTM D3418 |
E-Polymers EFLEX® M200 Ethylene Propylene Rubber M-series: E-FLEX M series resins are a maleic anhydride grafted (MAH) polymer concentrate designed as synthetic rubber and polyolefin manufactured by E-Polymers. It offers excellent adhesion to nyl.. |
|||
Melting Point | 53.0 °C | 127 °F | Freezing point via DSC/ASTM D3418 |
DuPont Bynel® 3859 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
(discontinued **) Bynel® Series 3800 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |