Material Notes:
DuPont™ Elvax® 3175LGA is an extrudable ethylene-vinyl acetate copolymer resin containing low gel material available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. ELVAX® 3175LGA EVA Resin complies with Food and Drug Administration Regulation 21 CFR 177.1350(a)(1) - - Ethylene-vinyl acetate copolymers, subject to the limitations and requirements therein. This Regulation describes polymers that may be used in contact with food, subject to the finished food-contact article meeting the extractive limitations under the intended conditions of use, as shown in paragraph (b)(1) of the Regulation.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ASTM D792, ISO 1183
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
Thermal Properties Metric English Comments
Melting Point 53.0 °C
127 °F
Freezing Point; ASTM D3418, ISO 3146
74.0 °C
165 °F
ASTM D3418, ISO 3146
Vicat Softening Point 43.0 °C
109 °F
ASTM D1525, ISO 306
Processing Properties Metric English Comments
Processing Temperature <= 230 °C
<= 446 °F
Melt Temperature 175 - 215 °C
347 - 419 °F
Extrusion Coating