Polymer Property : Melting Point = 4260 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 2350 °C
4260 °F
American Elements Europium Oxide Nanopwder
General DescriptionEU-MITE powders and dispersions are inorganic europium-oxide nanoparticles. EU-MITE-A products are uncoated and hydrophilic. EU-MITE-O products are coated with an organic silane (..