Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 39.0 - 41.0 °C | 102 - 106 °F | |
Oceanchem Group Antioxidant DLTP Molecular Formula: C30H58O4SCas No.: 123-28-4Characteristics and Uses: As a thioester auxiliary antioxidant with good performance, it is namely applied to polyethylene, polypropylene, PVC, AS resin,.. |