Polymer Property : Melting Point = 106 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 39.0 - 41.0 °C
102 - 106 °F
Oceanchem Group Antioxidant DLTP
Molecular Formula: C30H58O4SCas No.: 123-28-4Characteristics and Uses: As a thioester auxiliary antioxidant with good performance, it is namely applied to polyethylene, polypropylene, PVC, AS resin,..