Melting Point <= 4.00 °C
<= 39.2 °F
Freezing Point
Solvay MIRACARE® BC-27 Surfactant
Description: Specially formulated performance concentrate for ultra-mild skin cleansers, bubble baths, and shampoos for infant and geriatric markets. Provides non-irritating, tear-free cleansing and..
Melting Point 4.00 °C
39.2 °F
BASF Myristyl Chloroformate
Formula: C15H29ClO2CAS: 56677-60-2Description: Myristyl Chloroformate is a colorless to yellowish liquid with a pungent odor. Synonyms: Chloroformic acid tetradecyl ester, Carbonochloridic acid, tet..