Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | <= 4.00 °C | <= 39.2 °F | Freezing Point |
Solvay MIRACARE® BC-27 Surfactant Description: Specially formulated performance concentrate for ultra-mild skin cleansers, bubble baths, and shampoos for infant and geriatric markets. Provides non-irritating, tear-free cleansing and.. |
|||
Melting Point | 4.00 °C | 39.2 °F | |