Polymer Property : Melting Point = 3580 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 1970 °C
3580 °F
MarkeTech Yttrium aluminum garnet:Ce (YGA:Ce; Y3Al5O12) Scintillator Crystal
Yttrium aluminum garnet activated by cerium is fast with excellent mechanical properties and is chemically resistant scintillator. Mechanical properties enable to produce YAG:Ce scintillation screen..